Mechanical Properties Metric English Comments
Izod Impact, Unnotched 9.50 J/cm
17.8 ft-lb/in
ASTM D4812
Premix Premi-Glas® 3404 33% Glass Reinforced SMC
Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required...
Izod Impact, Unnotched 9.50 J/cm
17.8 ft-lb/in
J/cm²
Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber  (discontinued **)
Symbol according to ISO 1043/1: PBT+PC (GF) Elastomer modified PBT+PC blend reinforced with 5% of glass fibres, a good combination of stiffness, dimensional stability and thoughness. Main applicat..
Izod Impact, Unnotched 9.50 J/cm
17.8 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Izod Impact, Unnotched 9.50 J/cm
17.8 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12
LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber.
Izod Impact, Unnotched 9.50 J/cm

@Temperature -30.0 °C
17.8 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched 9.50 J/cm

@Temperature -30.0 °C
17.8 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched 9.50 J/cm

@Temperature -30.0 °C
17.8 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched 9.50 J/cm

@Thickness 3.18 mm
17.8 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..