Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043/1: PBT+PC (GF) Elastomer modified PBT+PC blend reinforced with 5% of glass fibres, a good combination of stiffness, dimensional stability and thoughness. Main application fields: automotive industry Filled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 250 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min
Elongation at Break 20 %
20 %
Nominal
Elongation at Yield 3.6 %
3.6 %
50 mm/min
Tensile Modulus 2.80 GPa
406 ksi
1 mm/min
Izod Impact, Unnotched 9.50 J/cm
17.8 ft-lb/in
J/cm²
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
Vicat Softening Point 123 °C
253 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in