Mechanical Properties Metric English Comments
Tensile Strength at Break 0.586 MPa
85.0 psi
Typical Value; ASTM D412
Parker Chomerics CHO-FORM 5532 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553..