Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.758 MPa | 110 psi | ASTM D412 |
Teknor Apex Telcar® TL 83-F943D22-NT Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 0.758 MPa | 110 psi | |
3M Interam™ E-5A-4 Endothermic Mat When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap.. |
|||
Tensile Strength at Break | 0.758 MPa @Temperature 121 °C |
110 psi @Temperature 250 °F |
|
3M Weatherban™ 606NF Acrylic Sealant 3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M.. |