Tensile Strength at Break 1.77 MPa
256 psi
Aearo E-A-R Specialty Composites Isoloss® VL Polyurethane Elastomer
Isoloss® VL elastomers have an extremely low modulus and good damping performance throughout a useful range of 0°C to 49°C. Isoloss® Polyurethane Elastomers feature high internal damping proper..