Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 793 MPa | 115000 psi | Bar |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Stress relieved |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Stress relieved |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Annealed |
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Annealed |
California Fine Wire Stablohm 875 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 790 MPa | 115000 psi | R<sub>m</sub>. 700°C tempering temperature. Quenching in oil ø 120. Testpiece hardened by oil quenching from 850°C. |
Assab Steels 705M Machinery Steel ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde.. |