Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 793 MPa | 115000 psi | Bar |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Stress relieved |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Stress relieved |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Annealed |
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 793 MPa | 115000 psi | Annealed |
California Fine Wire Stablohm 875 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |