Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 827 MPa | 120000 psi | |
Greene Tweed Xycomp® 1030-02 Carbon/Nylon 12 Composite Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |
|||
Tensile Strength at Break | 827 MPa | 120000 psi | Stress relieved |
California Fine Wire NIFE 5200 Nickel Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 827 MPa | 120000 psi | Annealed |
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 827 MPa | 120000 psi | Hard |
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80 Thickness >80-100 mm Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80 Thickness 16-80 mm Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80 Thickness 5 - Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80PV Thickness >80-100 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80PV Thickness 6- A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80PV Thickness 16-80 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength at Break | 827 MPa | 120000 psi | ASTM D638 |
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
(discontinued **) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |