Material Notes:
Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the high strength properties of BISPLATE 80 allows reduction in section thickness without loss of structural integrity.Applications: Transport Equipment, High Rise Buildings, Bridges, Excavator Buckets, Storage Tanks, Lifting Equipment, Mining Equipment, Induced Draft FansTesting: AS/NZS 3597 Grade 700 NATA approvedWelding: According to AS/NZS 1554 parts 4 and 5Tolerance: In accordance with AS/NZS 1365
Mechanical Properties Metric English Comments
Hardness, Brinell 255
255
Tensile Strength at Break 830 MPa
120000 psi
Tensile Strength, Yield 750 MPa

@Strain 0.200 %
109000 psi

@Strain 0.200 %
Elongation at Break 26 %
26 %
in 50 mm GL
Charpy Impact 160 J

@Temperature -20.0 °C
118 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Boron, B 0.0010 %
0.0010 %
Carbon, C 0.16 %
0.16 %
Chromium, Cr 0.90 %
0.90 %
Iron, Fe 97.4 %
97.4 %
As Balance
Manganese, Mn 1.15 %
1.15 %
Molybdenum, Mo 0.20 %
0.20 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0030 %
0.0030 %
Descriptive Properties Value Comments
CE (IIW) 0.58
PCM 0.3
Surface Finish Shotblasted