Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.7370 MPa | 1267.2 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 8.7370 MPa | 1267.2 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tensile Strength at Break | 8.7370 MPa | 1267.2 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |