Tensile Strength at Break 8.7370 MPa
1267.2 psi
Air at 302°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Tensile Strength at Break 8.7370 MPa
1267.2 psi
Air at 302°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
Tensile Strength at Break 8.7370 MPa
1267.2 psi
Air at 302°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..