Mechanical Properties Metric English Comments
Tensile Strength at Break 930 - 1100 MPa
135000 - 160000 psi
Schmolz + Bickenbach UGICHROM 4542 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 931 MPa
135000 psi
Hard
California Fine Wire Nickel A 200 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 931 MPa
135000 psi
Hard
California Fine Wire Nico Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.