Polymer Property : Tensile Strength at Break = 160000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 900 - 1100 MPa
131000 - 160000 psi
Schmolz + Bickenbach UGICHROM 4418 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 930 - 1100 MPa
135000 - 160000 psi
Schmolz + Bickenbach UGICHROM 4542 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 880 - 1100 MPa
128000 - 160000 psi
50<x=60mm
ThyssenKrupp XABO® 890 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength at Break 880 - 1100 MPa
128000 - 160000 psi
60<x=80mm
ThyssenKrupp XABO® 890 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength at Break 880 - 1100 MPa
128000 - 160000 psi
80<x=100mm
ThyssenKrupp XABO® 890 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength at Break 940 - 1100 MPa

@Thickness 50.0 mm
136000 - 160000 psi

@Thickness 1.97 in
ThyssenKrupp XABO® 890 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength at Break 970 - 1100 MPa
141000 - 160000 psi
50<x=60mm
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength at Break 650 - 1100 MPa
94300 - 160000 psi
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Information provided by Goodfellow.