Mechanical Properties Metric English Comments
Tensile Strength at Break >= 0.965 MPa
>= 140 psi
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Tensile Strength at Break 0.965 MPa
140 psi
ASTM D638
ExxonMobil ENABLE™ EN 33900 Adhesive and Sealant Applications Resin  (discontinued **)
Enable EN 33900 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical
Tensile Strength at Break 0.965 MPa
140 psi
ASTM D412
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 0.965 MPa
140 psi
ASTM D638
ExxonMobil EN 33900 Ethylene n-Butyl Acrylate Copolymer Resin
Product Description: ExxonMobil EN 33900 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive..
Tensile Strength at Break 0.965 MPa
140 psi
3M 4016 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Tensile Strength at Break 0.965 MPa
140 psi
3M 4056 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Tensile Strength at Break 0.965 MPa
140 psi
3M 4085 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..