Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 98.6 MPa | 14300 psi | ASTM D638 |
PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength at Break | 98.6 MPa | 14300 psi | ASTM D638 |
Chase Plastics CP Pryme® N213GL (DAM) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |