Mechanical Properties Metric English Comments
Tensile Strength at Break 1.00 - 3.00 MPa
145 - 435 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9510 Rubber-like Prototyping Polymer
Primary material: TangoGraySecondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide th..
Tensile Strength at Break >= 1.00 MPa
>= 145 psi
Sibur SKN-18SE Nitrile-Butadiene Rubber (NBR)
For production of rubber and asbestos technical articles which are used as sets for automobile, air planes, different machines and equipment, agricultural, drilling, and polygraph machinery, as well..
Tensile Strength at Break 1.00 MPa
145 psi
After Curing
Silikony Polskie Gumosil E Silicone Rubber
Very flexible with low hardness
Tensile Strength at Break 1.00 MPa
145 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 9H0600A
LNP* Thermocomp* 9H0600A is a High Specific Gravity compound containing proprietary fillers.
Tensile Strength at Break 1.00 MPa
145 psi
ASTM D638
Unitika elitel UE3231 Polyester, Flake
Molecular weight higher than UE3230, Improved solubilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as ad..
Tensile Strength at Break 1.00 MPa
145 psi
ASTM D412
3M 740 Hybrid Sealant
3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp..
Tensile Strength at Break 1.00 MPa

@Temperature 60.0 °C
145 psi

@Temperature 140 °F
3M Weatherban™ 606NF Acrylic Sealant
3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M..