Mechanical Properties Metric English Comments
Tensile Strength at Break 1640 MPa
238000 psi
Bisalloy Steels BisPlate 500 Thickness 6-100 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in sliding and gouging abrasion applications.Applications: Dump Truck Wear Liners, Chutes, Wear Liners, Earth Moving..
Tensile Strength at Break 1640 MPa
238000 psi
Bisalloy Steels BisPlate HHA Thickness 5-25 mm
A quenched and tempered steel armor plate suitable for use in both military and civil applications where light weight and resistance to ballistic projectiles is required.