Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.4 MPa | 1650 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R174AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene® RT-5180 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | Molded; ASTM D638 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | ASTM D638 |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | ASTM D412 |
Teknor Apex Monprene® MP-2465A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | ASTM D412 |
Teknor Apex Uniprene® 87A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | ASTM D412 |
Teknor Apex Uniprene® UN-2420B Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | ASTM D412 |
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Tensile Strength at Break | 11.4 MPa | 1650 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow FLEXOMER™ DFDB-9042 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-9042 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It has value as a sealant layer in multilayer film structures for dry and liquid packaging. I.. |