Material Notes:
FLEXOMER™ DFDB-9042 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It has value as a sealant layer in multilayer film structures for dry and liquid packaging. Information provided by Dow
Physical Properties Metric English Comments
Density 0.8985 g/cc
0.03246 lb/in³
ASTM D792
Melt Index of Compound 5.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
1 sec; molded and tested in accordance with ASTM D4976; ASTM D2240
93
93
5 sec; molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 11.4 MPa
1650 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 900 %
900 %
Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 0.117 GPa
17.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A
Thermal Properties Metric English Comments
Melting Point 119 °C
246 °F
Dow Method (DSC)
Glass Transition Temp, Tg -52.2 °C
-62.0 °F
Dow Method