Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 123 MPa | 17900 psi | ASTM D638 |
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties) Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 per.. |
|||
Tensile Strength at Break | 123 MPa | 17900 psi | ASTM D638 |
PlastxWorld CEVIAN® B5726 30% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Tensile Strength at Break | 123 MPa | 17900 psi | ASTM D638 |
Chase Plastics CP Pryme® NN133GL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 123 MPa | 17900 psi | ASTM D638 |
Chase Plastics CP Pryme® NN133GLUV (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated, UV Stabilized Information provided by Chase Plastics. |