Polymer Property : Tensile Strength at Break = 191 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 191 MPa
27700 psi
ASTM D638
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Tensile Strength at Break 191 MPa
27700 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include : Electrically Conductive.
Tensile Strength at Break 191 MPa
27700 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66
LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
Tensile Strength at Break 191 MPa
27700 psi
ASTM D 638
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific)
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength at Break 191 MPa
27700 psi
ASTM D 638
SABIC Innovative Plastics LNP Verton OX07411 PPS
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.