Polymer Property : Tensile Strength at Break = 198 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 198 MPa
28700 psi
ISO 527
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific)
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength at Break 198 MPa
28700 psi
ISO 527
SABIC Innovative Plastics LNP VERTON RX89047 PA 66
LNP* VERTON* RX89047 is a compound based on Nylon 66 resin containing Proprietary Fillers. Added feature of this grade is: Structural.
Tensile Strength at Break 198 MPa
28700 psi
ISO 527
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Asia Pacific)
LNP* Verton* RX89047 is a compound based on Nylon 66 resin.
Tensile Strength at Break 198 MPa
28700 psi
ISO 527
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East)
LNP* Verton* RX89047 is a compound based on Nylon 66 resin.
Tensile Strength at Break 198 MPa
28700 psi
ISO 527
SABIC Innovative Plastics LNP Verton OX07411 PPS
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.