Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Verton* RX89047 is a compound based on Nylon 66 resin.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
1.42 g/cc
0.0513 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 198 MPa
28700 psi
ISO 527
202 MPa
29300 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
198 %
198 %
ISO 527
Tensile Modulus 11.37 GPa
1649 ksi
50 mm/min; ASTM D638
Flexural Strength 317 MPa
46000 psi
ASTM D790
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
9.65 GPa
1400 ksi
ASTM D790
Izod Impact, Notched 3.57 J/cm
6.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.14 J/cm
19.00 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 251 °C
484 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
253 °C

@Thickness 3.20 mm
487 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved