Polymer Property : Tensile Strength at Break = 225 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 225 MPa
32600 psi
50 mm/min; ASTM D638
Ovation Polymers Opnyl OP6GF50 Nylon 6, 50% Glass Reinforced, Dry
Nylon 6 - Glass reinforced (50 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m..
Tensile Strength at Break 225 MPa
32600 psi
ASTM D638
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-1/-2
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber
PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates
Tensile Strength at Break 225 MPa
32600 psi
ISO 527 Type 1A
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY
Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is ..
Tensile Strength at Break 225 MPa
32600 psi
ISO R 527
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0
Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527
Solvay Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Tensile Strength at Break 225 MPa
32600 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 225 MPa
32600 psi
ISO 527
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66
LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b..
Tensile Strength at Break 225 MPa
32600 psi
ASTM D638
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-93
Wellman Wellamid® GFX1743-N1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6
Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman.
Tensile Strength at Break 225 MPa
32600 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-35 PA6-GF35
Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy..
Tensile Strength at Break 225 MPa
32600 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GC-4H PA*-CF40
Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo..
Tensile Strength at Break 225 MPa
32600 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSG-35 PA666-GF35
Information provided by EMS Grivory
Tensile Strength at Break 225 MPa
32600 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**)
43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Tensile Strength at Break 225 MPa
32600 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66  (Unverified Data**)
43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 225 MPa
32600 psi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Strength at Break 225 MPa
32600 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45
Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY ..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527
Eurotec® Tecomid® NA40 CR30 BK111 PA6.6, 30% carbon fiber reinforced, black
Information provided by Eurotec®
Tensile Strength at Break 225 MPa
32600 psi
ISO 527
Eurotec® Tecomid® NBX0 GR60 NL PA6, 60% glass fiber reinforced, natural
Information provided by Eurotec®
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-2
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-2
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-2
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-2
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
Tensile Strength at Break 225 MPa
32600 psi
ISO 527-2
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
Tensile Strength at Break 225 MPa
32600 psi
5 [mm/min]; ISO 527-1/2
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..