Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.62 MPa @Time 7200 sec |
235 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-9000 TPE Product Description: StarGrip GP 25-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubber.. |
|||
Tensile Strength at Break | 1.62 MPa @Time 1.21e+6 sec |
235 psi @Time 336 hour |
180°F (82°C) and then tested at 75°F (24°C) |
3M Weatherban™ 606NF Acrylic Sealant 3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M.. |