Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 240 MPa | 34800 psi | ASTM D638 |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ISO 527-1/-2 |
Lanxess Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV008S PA 66 LNP* VERTON* RV008S is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | ISO 527-1/-2 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50 Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | 5 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | 5 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Conditioned, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | |
BASF Ultramid® A3EG10 High Speed Information provided by BASF |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | 5 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Strength at Break | 240 MPa | 34800 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |