Tensile Strength at Break 244 MPa
35400 psi
ISO 527
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced  (discontinued **)
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Tensile Strength at Break 244 MPa
35400 psi
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Tensile Strength at Break 244 MPa
35400 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Tensile Strength at Break 244 MPa
35400 psi
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Tensile Strength at Break 244 MPa
35400 psi
ASTM D 638
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 244 MPa
35400 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.