Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.9 - 19.3 MPa | 2300 - 2800 psi | |
ITW Plexus Plexusâ„¢ MA821 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo.. |