Polymer Property : Tensile Strength at Break = 2960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.4 MPa
2960 psi
3M 5959 Outdoor Masking and Stucco Tape
3M™ Outdoor Masking and Stucco Tape 5959 has a high tensile strength backing for pulling through stucco, EIFS and other heavy coatings. Moisture and UV resistant, strong conformable backing. Clean ..
Tensile Strength at Break 20.4 MPa
2960 psi
ASTM D3759
3M Scotch® 4737S High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..
Tensile Strength at Break 20.4 MPa
2960 psi
ASTM D3759
3M Scotch® 4737T High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..