3M Scotch® 4737T High Temperature Fine Line Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 4737T High Temperature Fine Line Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.Information provided by 3M
Physical Properties Metric English Comments
Thickness 3.48 microns
0.137 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.4 MPa
2960 psi
ASTM D3759
Elongation at Break 115 %
115 %
ASTM D3759
Peel Strength 0.11504 kN/m
0.65625 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
for up to 30 mins
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Blue (Translucent)