Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.1 MPa | 3060 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3870 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 21.1 MPa | 3060 psi | 50 mm/min; ASTM D638 |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |
|||
Tensile Strength at Break | 21.1 MPa | 3060 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 6530 Antistatic Polystyrene Characteristics Prevents dust patterns due to static charges Eliminates need of coatings Fully colorable Processing Injection molding Extrusion & Forming Applications Meter housings Foodservice .. |
|||
Tensile Strength at Break | 21.1 MPa | 3060 psi | ISO 527-1/-2 |
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength at Break | 21.1 MPa | 3060 psi | ISO 527-1/-2 |
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |