Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 319 MPa | 46300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |