Mechanical Properties Metric English Comments
Tensile Strength at Break 319 MPa
46300 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK
LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.