Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 22.5 MPa | 3260 psi | ISO R 527 |
Stir SpA SG 78 K8 (PVC) Application: Extrusion pipes for conveying warm waterCold flex = -28°CInformation provided by STIR SpA |
|||
Tensile Strength at Break | >= 22.5 MPa | >= 3260 psi | |
Sibur SKN-33ASME Nitrile-Butadiene Rubber (NBR) For production of rubber and asbestos technical articles which are used as sets for automobile, air planes, different machines and equipment, agricultural, drilling, and polygraph machinery, as well.. |
|||
Tensile Strength at Break | 22.5 MPa | 3260 psi | |
3M Controltac™ IJ160C Graphic Film with Comply™ Adhesive 4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels .. |
|||
Tensile Strength at Break | 22.5 MPa | 3260 psi | |
3M Controltac™ IJ160 Graphic Film 4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels .. |