Material Notes:
4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels for fast, easy, bubble-free graphic installations; Excellent hiding power and Removable with heatInformation provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
without adhesive
114 - 127 microns
4.50 - 5.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.5 MPa
3260 psi
Peel Strength 0.158 kN/m
0.900 pli
Adhesion to Fruehauf pre-painted panels
0.578 kN/m
3.30 pli
Adhesion to ABS
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Minimum Service Temperature, Air 4.40 °C
39.9 °F
Copyright © lookpolymers.com All Rights Reserved