Polymer Property : Tensile Strength at Break = 3350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.1 MPa
3350 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R279AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D638
Teknor Apex APEX® 3600-90NT Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D638
Teknor Apex APEX® 3700-90 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D638
Teknor Apex APEX® 65001 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Features: Flame Retardant; Non-lead Uses: Communication Wire Jacketing Wire Types: CL2; CL3; CM; FPL; MP; OFN Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770;..
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D638
Teknor Apex APEX® 90-A471R-90-NT Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno..
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D638
Teknor Apex APEX® 65001 FOB Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D1708
GEHR Plastics ECOGEHR® WPC-30PE Composite of 70% Wood Fibers and 30% Polyethylene (PE)  (discontinued **)
Wood-polymer-composites (WPC) - these materials are composites of standard polymers and wood fibers. The excellent binding of the wood fibers to the polymer gives the materials extremely high mecha..
Tensile Strength at Break 23.1 MPa
3350 psi
ASTM D4745
3M Dyneon™ CC103 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company