Polymer Property : Tensile Strength at Break = 38.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.9 MPa
5640 psi
Indium Corp. Indalloy 258 Tin Solder Alloy
Information Provided by Indium Corporation
Tensile Strength at Break 38.9 MPa
5640 psi
ASTM D638
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength at Break 38.9 MPa
5640 psi
ASTM D638
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp
Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c..