Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 38.9 MPa | 5640 psi | |
Indium Corp. Indalloy 258 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Tensile Strength at Break | 38.9 MPa | 5640 psi | ASTM D638 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength at Break | 38.9 MPa | 5640 psi | ASTM D638 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |