Polymer Property : Tensile Strength at Break = 4.07 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.07 MPa
590 psi
510 mm/min; ASTM D412A
PolyOne Synprene™ RT-5155 RoHS Natural Styrene Butadiene Block Copolymer (SBC)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength at Break 4.07 MPa
590 psi
Heat Aged 24 hours at 600F
Malvern Minerals Sliastic 437 with 50% Novacite® L-207A Quartz Filler
Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company.
Tensile Strength at Break 4.07 MPa
590 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/..
Tensile Strength at Break 4.07 MPa
590 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ HTE 1106 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)