Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.07 MPa | 590 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene™ RT-5155 RoHS Natural Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 4.07 MPa | 590 psi | Heat Aged 24 hours at 600F |
Malvern Minerals Sliastic 437 with 50% Novacite® L-207A Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tensile Strength at Break | 4.07 MPa | 590 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/.. |
|||
Tensile Strength at Break | 4.07 MPa | 590 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1106 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) |