Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.79 - 4.14 MPa | 550 - 600 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1102 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Tensile Strength at Break | 3.45 - 4.14 MPa | 500 - 600 psi | |
Master Bond MasterSil 710 Silicone Paste Meets MIL Spec Description: MasterSil 710 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This product meets the Meets MIL-.. |