Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D638 |
Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP 1869 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1736R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1736S Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1829-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2260 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2260-R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2287M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2315C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2349 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 3.45 - 4.14 MPa | 500 - 600 psi | |
Master Bond MasterSil 710 Silicone Paste Meets MIL Spec Description: MasterSil 710 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This product meets the Meets MIL-.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D638 |
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesiv.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Metalfix-L™ Aluminum-Filled, Structural Adhesive Putty; Liquid Metalfix-L™ is a fluid-pourable version of MetalFix-P™. For patterns, molds, prototypes, casting, and all applications where a castable, fluid, MetalFix-P™ is needed. Excellent for tooling. Techn.. |