Tensile Strength at Break 425 MPa
61600 psi
Lengthwise; ASTM D638
G-9 Fiberglass Melamine Laminate Sheet
This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane..
Tensile Strength at Break 425 MPa
61600 psi
Lengthwise; ASTM D638
G-5 Fiberglass Melamine Laminate Sheet
This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and ..