Mechanical Properties Metric English Comments
Tensile Strength at Break 170 - 300 MPa
24700 - 43500 psi
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin..