Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Goodfellow Potassium Aluminosilicate (Muscovite Mica)

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Potassium Aluminosilicate (Muscovite Mica).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin micare, to shine or glitter. It can be split into thin uniform layers, down to 0.05 mm. The high skill involved in such splitting results in a high cost. Mica is transparent, and resistant to heat, as well as being one of the best electrical insulators known. It is resistant to high temperatures and chemically inert to most substances. It exhibits very low water absorption.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 2.60 - 3.20 g/cc
0.0939 - 0.116 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 2.0 - 3.0
2.0 - 3.0
Tensile Strength at Break 170 - 300 MPa
24700 - 43500 psi
Compressive Strength 190 - 280 MPa
27600 - 40600 psi
Shear Strength 215 - 265 MPa
31200 - 38400 psi
Thermal Properties Metric English Comments
CTE, linear 9.00 - 36.0 µm/m-°C

@Temperature 20.0 - 1000 °C
5.00 - 20.0 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 0.500 - 7.00 W/m-K
3.47 - 48.6 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 - 600 °C
932 - 1110 °F
Continuous
Optical Properties Metric English Comments
Refractive Index 1.50 - 1.60
1.50 - 1.60
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Dielectric Constant 6.0 - 6.6
6.0 - 6.6
Dielectric Strength 40.0 - 200 kV/mm
1020 - 5080 kV/in
Descriptive Properties Value Comments
Chemical Resistance - Alkalis Good
Chemical Resistance - Concentrated Acids Fair
Chemical Resistance - Dilute Acids Good
Users viewing this material also viewed the following: