Mechanical Properties Metric English Comments
Tensile Strength at Break 20.50 - 30.50 MPa
2973 - 4423 psi
ZCI-T-008
Zeon Chemicals Zetpol® 1020 Hydrogenated Nitrile Elastomomer
Zeptol 1020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance o..