Zeon Chemicals Zetpol® 1020 Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 1020 Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zeptol 1020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.Same as Zetpol 1010, except for lower saturation level allowing for sulfur cuing. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Iodine Absorption Number 20.3 - 28.5
20.3 - 28.5
mg/100mg; ZCI-T-004
Mooney Viscosity 71 - 85

@Temperature 100 °C
71 - 85

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 78
70 - 78
ZCI-T-009
Tensile Strength at Break 20.50 - 30.50 MPa
2973 - 4423 psi
ZCI-T-008
Elongation at Break 420 - 520 %
420 - 520 %
ZCI-T-008
300% Modulus 0.01340 - 0.01740 GPa
1.943 - 2.523 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD 91
Bound ACN (%, acrylonitrile) 42.9-45.5
Heat Loss (%) Max 0.5