Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.084 MPa | 737.3 psi | 302°F, 168 hr; ASTM D573 |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength at Break | 5.084 MPa | 737.3 psi | 302°F, 168 hr; ASTM D573 |
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |