Mechanical Properties Metric English Comments
Tensile Strength at Break 5.084 MPa
737.3 psi
302°F, 168 hr; ASTM D573
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength at Break 5.084 MPa
737.3 psi
302°F, 168 hr; ASTM D573
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..