Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE) Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Noble Polymers Ecobarrier™ 1512 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Tensile Strength at Break | 5.52 MPa | 801 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1101 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Tensile Strength at Break | 5.52 MPa | 801 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | Original; ASTM D638 |
LyondellBasell Petrothene® YR19513 Polyolefin Wire and Cable Compound ApplicationsPETROTHENE YR 19513 is a colorable, thermoplastic, non-halogenated, flame retardant polyolefin compound designed for use as striping for chemically crosslinkable automotive primary and a.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | Oven cured 4 hours at 480°F |
Malvern Minerals Sliastic 437 with 50% Novacite® Daper Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | >= 0.030" Thick |
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP1192A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP-1563 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP-1657L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP-2228C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP-2285CMT Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP-2745 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Monprene® MP-2830E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex Telcar® OBC 2318D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 5.52 - 6.21 MPa | 800 - 900 psi | |
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | 500 mm/min (20 in./min); ASTM-D638 Type IV Specimen |
Westlake EMAC® Plus SP1501 20% EMA Copolymer Westlake EMAC� Plus SP1501 is a 20% EMA copolymer designed for extrusion coating, compounding, and blending where low viscosity, flexibility, and strength are important. SP1501 provides excelle.. |
|||
Tensile Strength at Break | 5.52 MPa | 800 psi | Longitudinal; ASTM D882 |
Chesterton 850 Premium Sealing Tape Description: Chesterton® 850 Premium Sealing Tape is a high density, moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually .. |